Volume 6 • Issue 3 • 2015 • Fatigue and fracture

Articles


SCAD Journal Volume 6, Issue 3

Stijn Hertelé

2015-10-07 Volume 6 • Issue 3 • 2015 • Fatigue and fracture • 4

Characterisation of weld heterogeneity through hardness mapping and miniature tensile testing

Jonas Bally, Wim De Waele, Patricia Verleysen, Nenad Gubeljak and Stijn Hertelé

2015-10-07 Volume 6 • Issue 3 • 2015 • Fatigue and fracture • 8

Characterization of slip lines in single edge notched tension specimens

Filip Van Gerven, Wim De Waele, Diego Belato Rosado and Stijn Hertelé

2015-10-07 Volume 6 • Issue 3 • 2015 • Fatigue and fracture • 7

Evaluation of ductile tearing for API-5L X70 pipeline grade steel using SENT specimens

Nicholas Ohms, Diego Belato Rosado and Wim De Waele

2015-10-07 Volume 6 • Issue 3 • 2015 • Fatigue and fracture • 8

Testing methodologies for corrosion fatigue

Edward Delmotte, Nahuel Micone and Wim De Waele

2015-10-07 Volume 6 • Issue 3 • 2015 • Fatigue and fracture • 10

Effects of variable amplitude loading on fatigue life

Niels Laseure, Ingmar Schepens, Nahuel Micone and Wim De Waele

2015-10-07 Volume 6 • Issue 3 • 2015 • Fatigue and fracture • 10

The influence of material anisotropy and spiral welding on tensile strain capacity of spiral welded pipes

Michiel De Backer, Koen Van Minnebruggen and Wim De Waele

2015-10-07 Volume 6 • Issue 3 • 2015 • Fatigue and fracture • 9

Study of SENT specimens with a tilted notch to evaluate ductile tearing in spiral welded pipeline applications

Maxime Deprez, Frédéric Keereman, Koen Van Minnebruggen, Stijn Hertelé and Wim De Waele

2015-10-07 Volume 6 • Issue 3 • 2015 • Fatigue and fracture • 8

Low temperature tensile properties of line pipe steels

Harold Tubex, Koen Van Minnebruggen and Wim De Waele

2015-10-07 Volume 6 • Issue 3 • 2015 • Fatigue and fracture • 8